The settings for flux core wire and non ferrous metals will be completely different.
How to mig weld sheet metal flux core.
The flux cored arc welding uses similar or identical instruments use in mig inert metal gas welding.
The steel must be free from any rust paint or other contaminants.
This includes a flux cored welder welding gloves a welding mask safety goggles slag chipping hammer and a spool of flux core wire step 3 load the wire into the machine by following the proper instructions that came with your machine.
When welding mild steel a good rule of thumb is to set the amperage level at 1 amp for every 0 001 of thickness.
However flux cored arc welding can also be performed without shielding gas.
Subscribe for new videos every monday and friday.
For sheet metal i use ine welding wire and it is just as good as their flux cored wire if you want you can grab one here.
Clean it with a carbon steel wire brush.
Short bursts or tacks will help.
Although fcaw is known for being a process that can get away with welding dirty metal it is.
To weld sheet metal with solid wires use electrode positive ep or reverse polarity.
Don t attempt to weld thin materials like sheet metal with flux cored wires which put more heat into the base metal.
Metal thickness amperage settings.
So if you are welding 12 gauge mild steel with a thickness of 0 100 you would set the machine at 100 amps.
Basic guide to flux cored arc welding step 1.
It is also addressed as flux cored arc welding fcaw.
Https goo gl frdnss we continue to get tons of questions on some of the basics of flux cored welding.
You can use a stainless brush to clean with if that is all you have step 2 gather all your equipment.
Tig welding sheet metal forget the larger 1 8 inch tungsten electrode and use a smaller one.
Before you start welding you will need to make sure you have all the tools required.
Flux core is a welding process which uses a tubular wired electrode with a flux filled encore.